走進華晟 > 技術交流
1
|
290T春亞紡緘量工藝
|
30°
|
1.5 80°
|
1.0 120°
|
40′120°
|
1.5 60°
|
|
|
2
|
300T/310T春亞紡緘量工藝
|
30°
|
1.0 120°
|
60′120°
|
1.2 60°
|
|
|
|
3
|
240T/190T/260T春亞紡緘量工藝
|
30°
|
1.5 80°
|
1.2 120°
|
40′120°
|
1.5 60°
|
|
|
4
|
200克以下淺色春亞紡上色工藝
|
30°
|
0.8 80°
|
0.6 110°
|
1.0 125°
|
20′125°
|
1.5 60°
|
|
5
|
1000克以下中淺色春亞紡上色工藝
|
30°
|
0.8 80°
|
0.6 110°
|
10′110°
|
1.0 130°
|
40′130°
|
1.5 60°
|
6
|
春亞紡軍綠.深灰.鹹菜色上色工藝
|
30°
|
0.8 80°
|
0.6 115°
|
10′115°
|
1.0 130°
|
50′130°
|
1.5 60°
|
7
|
春亞紡芷青.特元上色工藝
|
30°
|
1.0 80°
|
0.7 110°
|
10′110°
|
1.0 130°
|
60′130°
|
1.5 60°
|
8
|
200克以下桃皮絨上色工藝
|
30°
|
0.8 80°
|
0.6 110°
|
1.0 125°
|
20′s125°
|
1.5 60°
|
|
9
|
1000克左右桃皮絨上色工藝
|
30°
|
0.8 80°
|
0.6 110°
|
10′110°
|
1.0 130°
|
40′130°
|
1.0 60°
|
10
|
5000克左右桃皮絨上色工藝
|
30°
|
0.9 80°
|
0.7 115°
|
10′115°
|
1.0 130°
|
60′130°
|
1.0 60°
|
11
|
桃皮絨芷青.黑色上色工藝
|
30°
|
1.0 80°
|
0.8 110°
|
10′110°
|
1.0 130°
|
60 130°
|
1.0 60°
|
12
|
消光塔絲隆緘量工藝
|
30°
|
1.0 105°
|
60′105°
|
1.0 60°
|
|
|
|
13
|
一般塔絲隆緘量工藝
|
30°
|
1.0 95°
|
60′95°
|
1.0 60°
|
|
|
|
14
|
消光塔絲隆淺色上色工藝
|
30°
|
0.5 70°
|
1.0 105°
|
40′105°
|
1.2 60°
|
|
|
15
|
消光.一般塔絲隆中色上色工藝
|
30°
|
0.5 70°
|
0.8 105°
|
60′105°
|
1.0 60°
|
|
|
16
|
消光.一般塔絲隆黑色.芷青上色工藝
|
30°
|
0.8 70°
|
1.0 105°
|
60′105°
|
1.0 60°
|
|
|
17
|
一般塔絲隆淺色上色工藝
|
30°
|
0.5 70°
|
1.0 95°
|
30′95°
|
1.2 60°
|
|
|
18
|
春亞紡.桃皮絨淺色特殊工藝
|
30°
|
0.8 80°
|
0.5 115°
|
10′115°
|
1.0 125°
|
40′125°
|
1.560°
|
19
|
春亞紡.桃皮絨深色特殊工藝
|
30°
|
0.8 80°
|
0.6 120°
|
10′120°
|
0.8 130°
|
60′130°
|
1.060°
|
20
|
春亞紡色花複修工藝
|
30°
|
3.5 135°
|
60′135°
|
1.5 60°
|
|
|
|
21
|
桃皮絨色花複修工藝
|
30°
|
3.5 135°
|
60′135°
|
1.0 60°
|
|
|
|
22
|
桃皮絨淺色煉布工藝
|
30°
|
3.0 120°
|
20′120°
|
2.060°
|
|
|
|
23
|
桃皮絨中深色煉布工藝
|
30°
|
2.0 110°
|
15′110°
|
2.0 60°
|
|
|
|
24
|
錦滌紡緘量工藝
|
30°
|
1.2 115°
|
40′115°
|
1.0 60°
|
|
|
|
25
|
錦滌紡淺色上色工藝
|
30°
|
0.6 80°
|
0.7 115°
|
15′115°
|
1.2 60°
|
|
|
26
|
錦滌紡中色上色工藝
|
30°
|
0.6 80°
|
0.7 110°
|
10′110°
|
1.0 120°
|
30′120°
|
1.0 60°
|
27
|
錦滌紡深色上色工藝
|
30°
|
0.8 80°
|
0.7 110°
|
10′110°
|
1.0 120°
|
50′120°
|
1.0 60°
|
28
|
幾皮絨淺色上色工藝
|
30°
|
1.3 80°
|
1.0 110°
|
10′110°
|
1.2 130°
|
40′130°
|
1.0 60°
|
29
|
幾皮絨深色上色工藝
|
30°
|
1.5 80°
|
1.0 110°
|
10′110°
|
1.2 130°
|
60′130°
|
1.0 60°
|
30
|
全滌斜桃煉白
|
30°
|
1.0 80°
|
10′80°
|
0.6 120°
|
40′120°
|
1.0 60°
|
|
31
|
斜桃煉白[精練]
|
30°
|
0.8 80°
|
10′80°
|
0.5 115°
|
1.0 130°
|
40′130°
|
1.0 60°
|
32
|
錦滌緞面開纖
|
30°
|
1.0 110°
|
80′110°
|
1.0 60°
|
|
|
|
33
|
錦滌緞面不開纖
|
30°
|
1.0 110°
|
50′110°
|
1.0 60°
|
|
|
|
34
|
錦滌斜紋開纖
|
30°
|
1.0 85°
|
10′85°
|
0.7 110°
|
60′110°
|
1.0 60°
|
|
35
|
錦滌斜紋不開纖
|
30°
|
1.0 80°
|
10′80°
|
0.7 110°
|
45′110°
|
1.0 60°
|
|
36
|
錦滌桃皮絨開纖
|
30°
|
1.0 80°
|
10′80°
|
0.7 110°
|
80′110°
|
1.0 60°
|
|
37
|
錦滌平紋開纖
|
30°
|
1.0 80°
|
10′80°
|
0.6 108°
|
60′108°
|
1.0 60°
|
|
38
|
錦滌平紋不開纖
|
30°
|
1.0 80°
|
10′80°
|
0.6 110°
|
50′110°
|
1.0 60°
|
|
39
|
經幾皮清水預縮
|
30°
|
1.0 80°
|
0.8 120°
|
30′120°
|
1.0 60°
|
|
|
40
|
緯幾皮煉白 30°1.2 60°
|
1.0 80°
|
10′80°
|
0.8 90°
|
60′90°
|
0.7 110°
|
15′110°
|
1.0 60°
|
41
|
經幾皮煉白 30°
|
1.0 80°
|
10′80°
|
0.8 90°
|
10′90°
|
0.7 105°
|
80′105°
|
1.0 60°
|
42
|
彈力經幾皮煉白 30°
|
1.0 80°
|
10′80°
|
0.8 90°
|
10′90°
|
0.7 105°
|
60′105°
|
1.0 60°
|
43
|
棉布打底
|
30°
|
0.5 65°
|
99′65°
|
1.0 50°
|
|
|
|
44
|
棉布緘量
|
30°
|
1.0 60°
|
60′60°
|
1.0 50°
|
|
|
|
45
|
桃皮絨緘量特殊工藝
|
30°
|
1.0 120°
|
40′120°
|
1.0 50°
|
|
|
|
46
|
幾皮中深色皂洗工藝
|
30°
|
1.0 80°
|
30′80°
|
1.0 60°
|
|
|
|
47
|
易绉經幾皮上色
|
|
10工藝130°*50′
|
|
|
|
|